Industrial Furnaces: Examples from real-life practice

Vacuum und protective gas soldering

Technology for Vacuum Soldering / Brazing

Pocess steps:

  • Loading, evacuating, heating, soldering, forced cooling and ready for a new use after in 4 hours
  • Separate Data recording for each process run
  • High availability
  • Best quality results coming from temperature homogeneity ± 3 K
  • Final vacuum better than 5x10-6 mbar
  • Accelerated processing with forced cooling at the process end
  • Cooling system on board (no cooling water installation)

Download PDF

 

Vakuumlöten und Schutzgaslöten

Powder manufacture

Rotary Furnaces DRF up to 1300°C

Process steps:

  • Adjusting the processing temperature
  • Adjusting the operating angle and rotation
  • Adjusting the material volume for heat treatment
  • Treating under air or protective gas
  • Transport vessels for transport under protective gas are available
  • Continuous operation

Download PDF

 

Pulverherstellung

General heat treatment in the laboratory

Vertical heat treatment furnace up to 1800°C

Specialities:

  • Drive in automatic (hot furnace)
  • Drive out automatic (hot furnace)
  • Drive out of the hot furnace
  • Quenching device
  • Up to 4 different gases
  • Hydrogen and carbon monoxid use
  • Sluice for charging
  • Continuous operation

Download PDF

Laborofen

Bridgman Crystal Growth Equipment

BV-HTRV 70-250/18 up to 1800°C

  • Frame with linear moving system
  • High temperature furnace HTRV 70-250/18
  • Ceramic tube 70x60 and vacuum-tight flanges
  • Rotary feed-through with pulling shaft and crucible holder
  • Drive unit with overdrive, pulling motor and rotation (option)
  • Sample thermocouple up to the top of the crucible
  • Control cabinet for drive unit and temperature control
  • Vacuum pumping unit (option)
  • Protective gas supply (option)
  • Data recording (option)

Download PDF